1)Use bulk limestone as raw material instead of powder limestone to reduce the cost.
2)The dryer is boil spray coating granulation which makes the process simple.
3)Temperature of inlet air is higher. Use high-temperature tail gas from the granulation dryer to concentrate the calcium chloride mother liquid. This technology not only recovery the waste heat but also solve the problem of removal dust. The whole process achieves maximum utilization of heat.